A reflow profile is not a single peak temperature — it is four zones doing four different jobs. Reading a curve means checking each zone against its own limit, with thermocouples on the board, not in the air.

Zone 1 — Preheat: get there without shocking the board

Preheat brings the assembly from room temperature to roughly 150 °C. The controlling number is ramp rate: about 3 °C/s maximum — fast enough to be productive, slow enough to avoid thermal shock to MLCCs and to let volatile solvents leave the paste gradually. Too fast gives solder spatter and beading; too slow exhausts the flux before reflow.

Zone 2 — Soak: stabilise before the melt

The soak plateau, typically 150–180 °C for 60–120 s, equalises temperature across the board so a heavy connector and an 0201 reach liquidus together, and lets flux activate and volatiles escape. Too short leaves a large delta-T and cold joints on thermal-mass parts; too long burns the flux, causing non-wetting and graping.

Zone 3 — Reflow: the only zone with a chemistry deadline

Above liquidus (217 °C for SAC305) the alloy melts and wets. Three numbers govern quality:

  • Peak temperature 235–245 °C — high enough to wet, low enough to limit intermetallic growth and component stress;
  • Time above liquidus 45–75 s — enough for wetting, not so long that IMC thickens and joints embrittle;
  • Peak dwell kept short, so the board does not soak at maximum temperature.

Nitrogen is optional for most consumer work and commonly justified on fine-pitch, high-reliability or low-void requirements.

Zone 4 — Cooling: where many "mystery" defects are born

Cooling rate should stay roughly 2–4 °C/s: too fast gives thermal shock, cracked joints and warpage; too slow coarsens the grain structure and reduces fatigue life. Cooling is also where BGA warpage and head-in-pillow risk is set.

Does every board need its own curve?

Yes, by thermal mass and paste type. A 1.6 mm six-layer controller board and a 2.4 mm compute board with a large heatsink pad cannot share a profile. Changing paste brand, oven, or a major component also requires a new profile.

How to accept a profile

  • Thermocouples attached to the board — at least one on the largest thermal mass, one on a small component, one near a BGA;
  • All four zones within limits, recorded with board ID and oven number;
  • Stored in MES and reused for repeat orders; re-measured on any change.
Profile measurement on the line: thermocouples on the board, four zones checked against limits

Profile measurement on the line: thermocouples on the board, four zones checked against limits

Ask for the profile record with your first article. A supplier who cannot produce one is guessing at the most consequential process in SMT.